SILK PLA
Glossy, satin-finish PLA blend that mimics painted plastic.
beginnerSpecialty
Specifications
Nozzle Temperature
210-220°C
Bed Temperature
50-65°C
Max Print Speed
60 mm/s
Drying Temp
45°C
Drying Time
4 hours
Enclosure
Not needed
Moisture Sensitive
No
Signs of Moisture
Watch for these signs
- loss of glossy sheen
- rough or matte surface
- popping during extrusion
- stringing
Storage Requirements
Temperature
15-25°C
Max Humidity
30% RH
Container
resealable bag with silica gel desiccant
Known Issues
Loses sheen if printed too cold
Cause: Polymer needs heat to develop the silk effect
Fix: Run 10°C hotter than standard PLA
Weaker layer bonding than PLA
Cause: Co-polymer additives reduce strength
Fix: Use only for cosmetic prints, not functional parts
Stringing on travel moves
Cause: Sticky melt
Fix: Increase retraction and add Z-hop
Best For
decorative prints and vasescosplay accentsmodels that look painted out of the printer
Not Good For
load-bearing partsfine miniatures (the sheen hides detail)outdoor parts
Compatible Build Surfaces
PEI
glass with glue stick
magnetic spring steel
Post-Processing Options
leave it - sheen is the appeal
light sanding only on bottom layers
Popular Brands
Brand-specific recommended temps and quirks. Click through for the full settings page.
61 brands found
Artillery
N 210°C B 60°C
View settings Eryone
N 230°C B 60°C
View settings Flashforge
N 210°C B 60°C
View settings 22 Network
N 210°C B 41°C
View settings 3D-Fuel
N 210°C B 60°C
View settings 3DJake
N 210°C B 60°C
View settings add:north
N 210°C B 60°C
View settings Amazon Basics
N 210°C B 60°C
View settings Ambrosia
N 205°C B 32°C
View settings American Filament
N 210°C B 60°C
View settings Amolen
N 210°C B 60°C
View settings Arianeplast
N 210°C B 60°C
View settings DIALED-IN SETTINGS
FixMyPrint generates exact slicer settings for Silk PLA- calibrated for your printer and slicer in seconds.
Generate Settings for Silk PLA